Home > Steel Surfaces CRP Experiments > R6106
Contact name | Makhlai | |
Steel type | Rusfer | |
Ion flux | φ /m-2.s-1 | 1e+22 |
Ion fluence | Γ /m-2 | 1e+26 |
Ion energy per D | E /eV | 30 – 1500 |
Sample thickness | t /mm | 1 |
Sample temperature | T /K | 500 |
Sample temperature measurement location | backside | |
Analysis method | mass loss | |
Sputtering yield | SY | 0.0024 |
Remarks | sample was coated by tungsten and irradiated by plasma streams before sputtered by ion beam |