Return to search
Plasma-Material Interaction Data Set 62
Solubility of H in CuCrZr
$$
K_\mathrm{s} = K_\mathrm{s0}\exp \left(-\frac{E_\mathrm{s}}{k_\mathrm{B}T}\right)
$$
[In the above formula, the Boltzmann constant is expressed in \(\mathrm{eV\,K^{-1}}\).]
- Material: CuCrZr
- Material composition: 0.65 wt% Cr, 0.1 wt% Zr
- Method: Experiment
- Data scaled for isotope mass? No
- Ks0 = 0.001 mol m-3 Pa-1/2
- Es = 0.0715 eV
- T = 573 – 873 K
Download JSON
- B6: S. Noh, W. Byeon, H. Shin, H. Kim, J. Kim, S. Lee, J. Kim, "Hydrogen-isotope transport in an ELBRODUR G CuCrZr alloy for nuclear applications in heat sinks
", Journal of Nuclear Materials 473, 112-118 (2016). [10.1016/j.jnucmat.2016.01.035]