Return to search

Plasma-Material Interaction Data Set 168

Permeation of D in Y2O3-Cr2O3

$$ P = P_0 \exp\left(-\frac{E_\mathrm{p}}{k_\mathrm{B}T}\right) $$

[In the above formula, the Boltzmann constant is expressed in \(\mathrm{eV\,K^{-1}}\).]

Comment

MOCVD followed by annealing at 1173K for composite. Data provided by M. Lavrentiev (UKAEA, 2024) with permission from STEP.

Download JSON

  1. B88: Y. Wu, D. He, S. Li, X. Liu, S. Wang, L. Jiang, "Deuterium permeation properties of Y2O3/Cr2O3 composite coating prepared by MOCVD on 316L stainless steel ", International Journal of Hydrogen Energy 41, 7425-7430 (2016). [10.1016/j.ijhydene.2016.03.132]