{"id":372,"qualified_id":"DM372","process":"Permeation","process_types":[{"abbreviation":"MPM","description":"Permeation"}],"method":"Experiment","scaled":false,"material":"Pd-25Ag","alloy":"","material_composition":"25%Pd, 75%Ag","species":{"qualified_id":"F3","text":"H","charge":0},"comment":"Data provided by Masashi Shimada (Idaho National Laboratories, USA, 2024).","refs":[{"qualified_id":"B134","authors":"E. Serra, M. Kemali, A. Perujo, D. K. Ross","title":"Hydrogen and deuterium in Pd-25 pct Ag alloy: Permeation, diffusion, solubilization, and surface reaction","journal":"Metallurgical and Materials Transactions A","volume":"29","page_start":"1023","page_end":"1028","year":1998,"doi":"10.1007/s11661-998-1011-3","bibcode":"1998MMTA...29.1023S","url":"https://dx.doi.org/10.1007/s11661-998-1011-3"}],"json_data":{"P0":{"value":5.58e-08,"units":"mol.m-1.s-1.Pa-1/2"},"Ep":{"value":0.06,"units":"eV"},"Trange":[323,773]}}