{"id":295,"qualified_id":"DM295","process":"Solubility","process_types":[{"abbreviation":"MSL","description":"Solubility"}],"method":"Experiment","scaled":false,"material":"Be","alloy":"","material_composition":"99.50%","species":{"qualified_id":"F4","text":"T","charge":0},"comment":"Solubility increases (exotermic behaviour); this might be due to traps, see Wampler1984. Data provided by M. Lavrentiev (UKAEA, 2024) with permission from STEP.","refs":[{"qualified_id":"B114","authors":"W. A. Swansiger","title":"Summary Abstract: Tritium solubility in high purity beryllium","journal":"Journal of Vacuum Science &amp; Technology A: Vacuum, Surfaces, and Films","volume":"4","page_start":"1216","page_end":"1217","year":1986,"doi":"10.1116/1.573400","bibcode":"1986JVSTA...4.1216S","url":"https://dx.doi.org/10.1116/1.573400"}],"json_data":{"Ks0":{"value":5900.0,"units":"mol.m-3.Pa-1/2"},"Es":{"value":1,"units":"eV"},"Trange":[713,783]}}