{"id":21,"qualified_id":"DM21","process":"Diffusivity","process_types":[{"abbreviation":"MDF","description":"Diffusion"}],"method":"Experiment","scaled":true,"material":"CuCrZr","alloy":"","material_composition":"0.65 wt% Cr, 0.05 wt% Zr","species":{"qualified_id":"F4","text":"T","charge":0},"comment":"Value of D0 for T scaled from that of H given in the cited reference by 1/sqrt(3).","refs":[{"qualified_id":"B24","authors":"I. Peñalva, G. Alberro, F. Legarda, G. A. Esteba, B. Riccardi","title":"Copper Alloys - Early Applications and Current Performance - Enhancing Processes","journal":"Interaction of Copper Alloys with Hydrogen","year":2012,"note":"Ed. Luca Collini","doi":"10.5772/34469","url":"https://www.intechopen.com/books/copper-alloys-early-applications-and-current-performance-enhancing-processes/interaction-of-copper-alloys-with-hydrogen"}],"json_data":{"D0":{"value":2.05e-05,"units":"m2.s-1"},"Ed":{"value":0.679,"units":"eV"},"Trange":[593,773]}}