{"id":12,"qualified_id":"DM12","process":"Recombination","process_types":[{"abbreviation":"MRC","description":"Recombination"}],"method":"Experiment","scaled":true,"material":"Cu","alloy":"","species":{"qualified_id":"F1","text":"D","charge":0},"comment":"Using oxygen-free high conductivity (OHFC) Cu flat stock. Note error in units for Kr0 of OFHC-Cu in the text of p.764 (m2/s should be m4/s).","refs":[{"qualified_id":"B13","authors":"R. Anderl, M. Hankins, G. Longhurst, R. Pawelko","title":"Deuterium transport in Cu, CuCrZr, and Cu/Be","journal":"Journal of Nuclear Materials","volume":"266-269","page_start":"761","page_end":"765","year":1999,"doi":"10.1016/s0022-3115(98)00878-2","bibcode":"1999JNuM..266..761A","url":"https://dx.doi.org/10.1016/S0022-3115(98)00878-2"}],"json_data":{"Kr0":{"value":9.1e-18,"units":"m4.s-1"},"Er":{"value":0.99,"units":"eV"},"Trange":[700,800]}}