Home > Recombination of Hydrogen on Metal Surfaces > Recombination of Deuterium on CuCrZr Alloys
Parameters for recombination of deuterium on copper-chromium-zirconium alloy surfaces.
Material Surface | CuCrZr | |
Recombination temperature dependence formula | $$K_r = K_{r0}\exp\left(-\frac{E_\mathrm{r}}{k_\mathrm{B}T}\right)$$ |
1 / 1 records shown.
pk | Composition | T /K | Kr0 /m4 s-1 | Er /eV | Note |
---|---|---|---|---|---|
R77 | 1.1% Cr, 0.1% Zr | 700 – 800 | 2.9e-14 | 1.92 | Deuterium transport in Cu, CuCrZr, and Cu/Be, Journal of Nuclear Materials 266±269 (1999) 761±765 |